| 廠家及牌號(hào) | 試驗(yàn)條件 | 測(cè)試方法 | 熔體流動(dòng)速率 |
| EMA ?松梨 TC 115 Blown (熱穩(wěn)定) | 190℃/2.16kg | ASTM D-1238 | 0.7 g/10min |
| EMA 美國(guó)西湖 SP2255 (擠出共聚物,較好的韌性,應(yīng)力裂紋抗拒,低溫韌性,軟) | 190℃/2.16kg | ASTM D-1238 | 2.1 g/10min |
| EMA 美國(guó)西湖 SP2258 (擠出共聚物,較好的韌性,應(yīng)力裂紋抗拒,低溫韌性,軟) | 190℃/2.16kg | ASTM D-1238 | 2.1 g/10min |
| EMA 美國(guó)西湖 SP1358 (擠出共聚物,較好的韌性,應(yīng)力裂紋抗拒,低溫韌性,軟) | 190℃/2.16kg | ASTM D-1238 | 2.4 g/10min |
| 此文獻(xiàn)-版權(quán)所有-請(qǐng)勿轉(zhuǎn)載或其它用途.http://www.melanomaexpert.com/ | |||
| EMA ?松梨 TC 114 Blown (熱穩(wěn)定) | 190℃/2.16kg | ASTM D-1238 | 3.2 g/10min |
| EMA 美國(guó)西湖 SP2242 (擠出共聚物,較好的韌性,應(yīng)力裂紋抗拒,低溫韌性,軟) | 190℃/2.16kg | ASTM D-1238 | 3.5 g/10min |
| EMA 美國(guó)西湖 SP2261 (擠出共聚物,較好的韌性,應(yīng)力裂紋抗拒,低溫韌性) | 190℃/2.16kg | ASTM D-1238 | 2.5 g/10min |
| EMA ?松梨 TC 110 Blown (熱穩(wěn)定) | 190℃/2.16kg | ASTM D-1238 | g/10min |
| EMA ?松梨 TC 114 Cast (熱穩(wěn)定) | 190℃/2.16kg | ASTM D-1238 | 3.2 g/10min |
| EMA 美國(guó)西湖 SP2252 (擠出共聚物,較好的韌性,應(yīng)力裂紋抗拒,低溫韌性,軟) | 190℃/2.16kg | ASTM D-1238 | 0.7 g/10min |
| 溫馨提示 | |||
| 1.有關(guān)“熔體流動(dòng)速率 EMA”類數(shù)據(jù)資訊最多展示10條.更多牌號(hào)應(yīng)用數(shù)據(jù)請(qǐng)向客服索取。 2.有關(guān)“EMA塑料顆粒價(jià)格”類數(shù)據(jù)的實(shí)時(shí)性及更多塑料顆粒價(jià)格行情敬請(qǐng)關(guān)注我們的資訊動(dòng)態(tài). | |||